5 Common Mistakes When Applying Microcement

5 Common Mistakes When Applying Microcement

5 Common Mistakes and How to Avoid Them

❌ Mistake #1: Insufficient Priming

If the surface absorbs primer like a sponge, apply a second coat. PRIMER Q should create an even layer, not a dry film.

❌ Mistake #2: Layers Too Thick

Microcement must be applied in thin layers (1-2 mm). Thick layers will crack and take longer to dry.

❌ Mistake #3: Not Enough Drying Time Between Coats

4-6 hours is the minimum. If you rush, the next coat may lift the previous one.

❌ Mistake #4: Forgetting to Mix the Varnish Properly

PU 2K VARNISH is two-component – mix A and B thoroughly! 3 minutes with a slow mixer.

❌ Mistake #5: Using the Surface Too Soon

Full curing takes 7 days. Be gentle before that!